{"paper":{"title":"Sub-micrometer yttrium iron garnet LPE films with low ferromagnetic resonance losses","license":"http://creativecommons.org/licenses/by-nc-sa/4.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"Andreas Danilewsky, Carsten Dubs, Jan Dellith, Oleksii Surzhenko, Ralf Linke, Uwe Br\\\"uckner","submitted_at":"2016-08-29T13:29:23Z","abstract_excerpt":"Using liquid phase epitaxy (LPE) technique (111) yttrium iron garnet (YIG) films with thicknesses of ~100 nm and surface roughnesses as low as 0.3 nm have been grown as a basic material for spin-wave propagation experiments in microstructured waveguides. The continuously strained films exhibit nearly perfect crystallinity without significant mosaicity and with effective lattice misfits of delta a(perpendicular)/a(substrate) ~10-4 and below. The film/substrate interface is extremely sharp without broad interdiffusion layer formation. All LPE films exhibit a nearly bulk-like saturation magnetiza"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1608.08043","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}