{"paper":{"title":"Large thermopower in the antiferromagnetic semiconductor BaMn$_2$Bi$_2$","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":["cond-mat.mtrl-sci"],"primary_cat":"cond-mat.str-el","authors_text":"C. Petrovic, Kefeng Wang","submitted_at":"2016-04-18T19:59:46Z","abstract_excerpt":"We report electrical and thermal transport properties of Mn-based material BaMn$_2$Bi$_2$ with ThCr$_2$Si$_2$ structure. The resistivity of the antiferromagnetic BaMn$_2$Bi$_2$ shows a metal-semiconductor transition at $\\sim 80$ K with decreasing temperature. Correspondingly, the thermopower $S$ shows a peak at the same temperature, approaching ~150 $\\mu$V/K. With increasing temperature $S$ decreases to about 125 $\\mu$V/K at the room temperature. The magnetic field enhances the peak value to 210 $\\mu$V/K. The Hall resistivity reveals an abrupt change of the carrier density close to the metal-s"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1604.05296","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}