{"paper":{"title":"Thermal Sublimation: a Scalable and Controllable Thinning Method for the Fabrication of Few-Layer Black Phosphorus","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"Guangrui (Maggie) Xia, Jialun Liu, Rui Yang, Weijun Luo, Wenjuan Zhu, Yunlong Zhao","submitted_at":"2016-01-16T00:53:36Z","abstract_excerpt":"In this work, we reported uniform layer-by-layer sublimation of black phosphorus under heating below 600 K. The uniformity and crystallinity of BP samples after thermal thinning were confirmed by Raman spectra and 2D Raman imaging. A uniform and crystalline bilayer black phosphorus flake with an area of 180 um^2 was prepared with this method. No micron scale defects were observed. The sublimation rate of BP was around 0.18 nm / min at 500 K and 1.5 nm / min at 550 K. Both room and high temperature Raman peak intensity ratio Si/A2g vs. BP thickness relations were established for in-situ thickne"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1601.04103","kind":"arxiv","version":4},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}