{"paper":{"title":"Characteristics of Nickel Thin Film and Formation of Nickel Silicide by Remote Plasma Atomic Layer Deposition using Ni(iPr-DAD)2","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"Heeyoung Jeon, Hyeongtag Jeon, Hyunjung Kim, Jingyu Park, Jinho Kim, Junhan Yuh, Woochool Jang","submitted_at":"2014-08-06T12:02:06Z","abstract_excerpt":"In this study, the characteristics of nickel thin film deposited by remote plasma atomic layer deposition (RPALD) on p-type Si substrate and formation of nickel silicide using rapid thermal annealing were determined. Bis(1,4-di-isopropyl-1,3-diazabutadienyl)nickel, Ni(iPr-DAD)2, was used as a Ni precursor and ammonia plasma was used as a reactant. This was the first attempt to deposit Ni thin film using Ni(iPr-DAD)2 as a precursor for the ALD process. The RPALD Ni film was deposited with a growth rate of around 2.2{\\AA}/cycle at 250 {\\deg}C and showed significant low resistivity of 33 {\\mu}{\\O"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1408.1252","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}