{"paper":{"title":"LaCrO3 heteroepitaxy on SrTiO3(001) by molecular beam epitaxy","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"L. Qiao, M.E. Bowden, S. A. Chambers, T.C. Droubay, T.C. Kaspar, V.Shutthanandan","submitted_at":"2011-05-21T20:54:54Z","abstract_excerpt":"Stoichiometric, epitaxial LaCrO3 films have been grown on TiO2-terminated SrTiO3(001) substrates by molecular beam epitaxy using O2 as the oxidant. Film growth occurred in a layer-by-layer fashion, giving rise to structurally excellent films and surfaces which preserve the step-terrace structure of the substrate. The critical thickness is in excess of 500 {\\AA}. Near-surface Cr(III) is highly susceptible to further oxidation to Cr(V), leading to the formation of a disordered phase upon exposure to atomic oxygen. Recovery of the original epitaxial LaCrO3 phase is readily achieved by vacuum anne"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1105.4290","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}