{"paper":{"title":"Evolution Process of Wurtzite ZnO Films on Cubic MgO (001) Substrates: a Structural, Optical and Electronic Investigation of the Misfit Structures","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"Hua Zhou, Hui-Qiong Wang, Jin-Cheng Zheng, Junyong Kang, Kim Kisslinger, Lihua Zhang, Lijun Wu, Yaping Li, Yimei Zhu, Yuying Huang, Zheng Jiang","submitted_at":"2014-05-07T21:26:43Z","abstract_excerpt":"The interface between hexagonal ZnO films and cubic MgO (001) substrates, fabricated through molecular beam epitaxy, are thoroughly investigated. X-ray diffraction and (scanning) transmission electron microscopy reveal that, at the substrate temperature above 200 degree C, the growth follows the single [0001] direction; while at the substrate below 150 degree C, the growth is initially along [0001] and then mainly changes to [0-332] variants beyond the thickness of about 10 nm. Interestingly, a double-domain feature with a rotational angle of 30 degree appears for the growth along [0001] regar"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1405.1757","kind":"arxiv","version":2},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}