{"paper":{"title":"Effects of post-deposition annealing on the structure and magnetization of PLD grown Yttrium Iron Garnet films","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"physics.app-ph","authors_text":"Ravinder Kumar, R. C. Budhani, Z. Hossain","submitted_at":"2019-03-22T11:40:25Z","abstract_excerpt":"We report on the recrystallization of 200 nm thick as-grown Yttrium Iron Garnet (Y_3.4 Fe_4.6 O_12) films on (111) face of Gadolinium Gallium Garnet (GGG) single crystals by post-deposition annealing. Epitaxial conversion of the as-grown microcrystalline YIG films was seen after annealing at 800oC for more than 30 minutes both in ambient oxygen as well as in air. The as-grown oxygen annealed samples at 800oC for 60 minutes crystallize epitaxially and show excellent figure-of-merit for saturation magnetization (MS = 3.3 {\\mu}B/f.u., comparable to bulk value) and coercivity (HC ~ 1.1 Oe). The am"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1903.09457","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}