{"paper":{"title":"Influence of homo-buffer layer on stress control of sputtered (Ba0.45,Sr0.55)TiO3 thin films on Pt-Si","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"Guillaume Guegan, Mohamed Lamhamdi, Patrick Simon, Virginie Grimal, Y.K. Vayunandana Reddy","submitted_at":"2013-09-06T12:09:09Z","abstract_excerpt":"To engineer strain relaxation of sputtered BST thin films on Pt-Si wafers, homo-buffer layer method was applied to eliminate Pt hillock formation. Thin BST homo-buffer layers were deposited at room temperature and subsequently the main BST layer was deposited at 650{\\deg}C, Pt hillock free BST films were obtained with homo-buffer thickness above 5 nm. Relatively good electrical properties were obtained for BST thin films with 15 and 25 nm homo-buffer layer (T= 30 % at 5V and tan {\\delta}= 0.018)."},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1309.1615","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}