{"paper":{"title":"Magnetocaloric effect in Gd/W thin film heterostructures","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mes-hall","authors_text":"Casey W. Miller, D. V. Williams, H. Srikanth, N. S. Bingham","submitted_at":"2011-12-15T22:10:48Z","abstract_excerpt":"In an effort to understand the impact of nanostructuring on the magnetocaloric effect, we have grown and studied gadolinium in MgO/W(50 $\\textrm{\\AA}$)/[Gd(400 $\\textrm{\\AA}$)/W(50 $\\textrm{\\AA}$)]$_8$ heterostructures. The entropy change associated with the second order magnetic phase transition was determined from the isothermal magnetization for numerous temperatures and the appropriate Maxwell relation. The entropy change peaks at a temperature of 284 K with a value of approximately 3.4 J/kg-K for a 0-30 kOe field change; the full width at half max of the entropy change peak is about 70 K,"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1112.3684","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}