{"paper":{"title":"Electrical transport and thermoelectric properties of silver nanoparticles","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mes-hall","authors_text":"Gunadhor Singh Okram, Vikash Sharma","submitted_at":"2019-08-20T13:43:25Z","abstract_excerpt":"Debye temperature decrease, residual resistivity increase and electron-phonon coupling constant increase as crystallite size decreases have been found from electrical resistivity in temperature range 5 K to 300 K of well-characterized Ag nanoparticles synthesized with oleylamine, trioctylphosphine and/ polyvinylpyrrolidone with Scherrer sizes ranging from 15.1 nm to 33.4 nm. Notably, about 36 % reduction in Debye temperature in 15.1 nm compared to bulk Ag is found. Remarkably, usual phonon drag peak found in Seebeck coefficient for bulk Ag turned into dips or phonon drag minima in these NPs th"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1908.07339","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"integrity":{"clean":true,"summary":{"advisory":0,"critical":0,"by_detector":{},"informational":0},"endpoint":"/pith/1908.07339/integrity.json","findings":[],"available":true,"detectors_run":[],"snapshot_sha256":"c28c3603d3b5d939e8dc4c7e95fa8dfce3d595e45f758748cecf8e644a296938"},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}