{"paper":{"title":"Giant magnetostriction in Tb-doped Fe83Ga17 melt-spun ribbons","license":"http://creativecommons.org/licenses/by-nc-sa/3.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"Chengbao Jiang, Huibin Xu, Jinghua Liu, Wei Wu","submitted_at":"2013-07-09T09:45:17Z","abstract_excerpt":"Giant magnetostriction is achieved in the slightly Tb-doped Fe83Ga17 melt-spun ribbons. The tested average perpendicular magnetostriction is -886 ppm along the melt-spun ribbon direction in the Fe82.89Ga16.88Tb0.23 alloy. The calculated parallel magnetostriction is 1772 ppm, more than 4 times as large as that of binary Fe83Ga17 alloy. The enhanced magnetostriction should be attributed to a small amount of Tb solution into the A2 matrix phase during rapid solidification. The localized strong magnetocrystalline anisotropy of Tb element is suggested to cause the giant magnetostriction."},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1307.2385","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}