{"paper":{"title":"Superconductivity phase diagram of Se-substituted CeO0.5F0.5Bi(S1-xSex)2","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.supr-con","authors_text":"Osuke Miura, Takafumi Hiroi, Yoshikazu Mizuguchi","submitted_at":"2015-11-12T06:02:12Z","abstract_excerpt":"We investigated the effects of Se substitution on the lattice constants and superconducting properties of CeO0.5F0.5Bi(S1-xSex)2. With increasing Se concentration, the a lattice constant increased, while the c lattice constant did not show any significant increase between x = 0.1 and x = 0.5. Bulk superconductivity was observed in samples with x = 0.2-0.4, and the superconducting transition temperature was the highest at x = 0.3. The obtained superconductivity phase diagram was compared to those of LaO0.5F0.5Bi(S1-xSex)2 and NdO0.5F0.5Bi(S1-xSex)2."},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1511.03787","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}