{"paper":{"title":"Current-driven domain wall motion across a wide temperature range in a (Ga,Mn)(As,P) device","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":["cond-mat.mes-hall"],"primary_cat":"cond-mat.mtrl-sci","authors_text":"A. C. Irvine, A. W. Rushforth, B. L. Gallagher, C. T. Foxon, D. A. Williams, E. De Ranieri, G. Tatara, J. Wunderlich, K. Olejnik, K. W. Edmonds, K. Y. Wang, R. P. Campion","submitted_at":"2010-05-06T09:34:56Z","abstract_excerpt":"Current-driven magnetic domain wall motion is demonstrated in the quaternary ferromagnetic semiconductor (Ga,Mn)(As,P) at temperatures well below the ferromagnetic transition temperature, with critical currents of the order 10^5Acm^-2. This is enabled by a much weaker domain wall pinning compared to (Ga,Mn)As layers grown on a strain-relaxed buffer layer. The critical current is shown to be comparable with theoretical predictions. The wide temperature range over which domain wall motion can be achieved indicates that this is a promising system for developing an improved understanding of spin-t"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1005.0946","kind":"arxiv","version":2},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}