{"paper":{"title":"Dielectric Investigation, Piezoelectric Measurement and Structural Studies of Strontium-doped, modified PMS-PZT Piezoelectric Ceramics","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"A. K. Himanshu, Kumar Brajesh, N. K. Singh, Rajeev Ranjan, Rajyavardhan Ray, S. K. Bandyopadhayay, T P Sinha, Yashwant Kumar","submitted_at":"2013-09-26T09:05:38Z","abstract_excerpt":"The structure and dielectric properties of 6% $\\rm{Sr}^{2+}$-substituted, modified Lead Zirconium Titanate (PZT) piezoelectric ceramic, with composition $[\\rm{Pb}_{0.94}\\rm{Sr}_{0.06}][(\\rm{Mn}_{1/3}\\rm{Sb}_{2/3})_{0.05}(\\rm{Zr}_{0.54}\\rm{Ti}_{0.46})_{0.95}]O_3$ and lead manganese antimonite as an additional dopant, synthesized by ceramic route have been investigated in a frequency range from 50Hz to 1MHz and in a temperature range between room temperature and 633K. The scanning electron micrograph of the sample taken at the room temperature confirms the formation of a fairly homogenous struct"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1309.6764","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}