{"paper":{"title":"Valency Configuration of Transition Metal Impurities in ZnO","license":"","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"A. Janotti, A. Svane, L. Petit, T.C. Schulthess, W.M. Temmerman, Z. Szotek","submitted_at":"2006-06-15T14:51:07Z","abstract_excerpt":"We use the self-interaction corrected local spin-density approximation to investigate the ground state valency configuration of transition metal (TM = Mn, Co) impurities in n- and p-type ZnO. We find that in pure Zn1-xTMxO, the localized TM2+ configuration is energetically favored over the itinerant d-electron configuration of the local spin density (LSD) picture. Our calculations indicate furthermore that the (+/0) donor level is situated in the ZnO gap. Consequently, for n-type conditions, with the Fermi energy eF close to the conduction band minimum, TM remains in the 2+ charge state, while"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"cond-mat/0606417","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"integrity":{"clean":true,"summary":{"advisory":0,"critical":0,"by_detector":{},"informational":0},"endpoint":"/pith/cond-mat/0606417/integrity.json","findings":[],"available":true,"detectors_run":[],"snapshot_sha256":"c28c3603d3b5d939e8dc4c7e95fa8dfce3d595e45f758748cecf8e644a296938"},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}