{"paper":{"title":"Broadband dielectric spectroscopy of mixed $CuInP_2(S_xSe_{1-x})_6$ crystals","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":["cond-mat.other"],"primary_cat":"cond-mat.mtrl-sci","authors_text":"J.Banys, J.Macutkevic, R. Grigalaitis, Yu. Vysochanskii","submitted_at":"2008-05-08T07:01:58Z","abstract_excerpt":"In this article mixed CuInP$_2$(S$_x$Se$_{1-x}$)$_6$ crystals were investigated by broadband dielectric spectroscopy (20 Hz - 3 GHz). The complete phase diagram has been obtained from these results. The phase diagram of investigated crystals is strongly asymmetric - the decreasing of ferroelectric phase transition temperatures in CuInP$_2$(S$_x$Se$_{1-x}$)$_6$ is much more flat with small admixture of sulphur then with small admixture of selenium. In the middle part of the phase diagram (x=0.4-0.9) the dipolar glass phase has been observed. In boundary region between ferroelectric order and di"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"0805.1109","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}