{"paper":{"title":"Stimulated emission from ZnO thin films with high optical gain and low loss","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"A-S. Gadallah, C. Couteau, D. J. Rogers, G. L\\'erondel, K. Nomenyo","submitted_at":"2013-07-13T09:55:52Z","abstract_excerpt":"Stimulated surface- and edge-emission were investigated for ZnO thin films grown epitaxially by pulsed laser deposition. The lasing threshold was 0.32 MW/cm2 for surface pumping and 0.5 MW/cm2 for edge pumping, which is significantly lower than thresholds observed previously. A modified variable stripe length method was used to measure the gain, which was 1369 cm-1 for N-band emission. Losses were measured using the shifting excitation spot method and values of 6.2 cm-1 and 6.3 cm-1 were found for the N-band and P-band, respectively. The measured gain and loss were the highest and lowest (resp"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1307.3636","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}