{"paper":{"title":"Radon Daughter Plate-out Measurements at SNOLAB for Polyethylene and Copper","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"astro-ph.IM","authors_text":"Ben Loer, Dan Bauer, Jodi Cooley, Matthew Stein, Ray Bunker, Rob Calkins, Silvia Scorza","submitted_at":"2017-08-30T21:16:17Z","abstract_excerpt":"Polyethylene and copper samples were exposed to the underground air at SNOLAB for approximately three months while several environmental factors were monitored. Predictions of the radon-daughter plate-out rate are compared to the resulting surface activities, obtained from high-sensitivity measurements of alpha emissivity using the XIA UltraLo-1800 spectrometer at SMU. From these measurements, we determine an average $^{210}$Pb plate-out rate of 249 and 423 atoms/day/cm$^{2}$ for polyethylene and copper, respectively, when exposed to radon activity of 135 Bq/m$^{3}$ at SNOLAB. A time-dependent"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1708.09476","kind":"arxiv","version":4},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}