{"paper":{"title":"Mechanical properties of electrodeposited amorphous/crystalline multilayer structures in the Fe-P system","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"Andrea Bachmaier, Reinhard Pippan, Ruth Konetschnik, Thomas Schoeberl, Timo Mueller","submitted_at":"2018-12-13T13:06:21Z","abstract_excerpt":"Amorphous/crystalline multilayer structures of Fe-P alloys were deposited electrochemically using the single bath technique. Hall-Petch behavior of microhardness with respect to sublayer thickness was observed down to a sublayer thickness of 15 nm. For thinner sublayers, a hardness plateau was obtained. The transition at a sublayer thickness of 15 nm coincides with the loss of the multilayer structure as observed in transmission electron microscopy. The transition is a possible result of a change in the amorphous to crystalline sublayer thickness ratio and the interface roughness development d"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1812.05404","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}