{"paper":{"title":"Measurements of Surface Diffusivity and Coarsening During Pulsed Laser Deposition","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"A.R. Woll, D.S. Dale, G. Arikan, J.D. Brock, J.D. Ferguson","submitted_at":"2009-10-19T15:50:25Z","abstract_excerpt":"Pulsed Laser Deposition (PLD) of homoepitaxial SrTiO3 <001> was studied with in-situ x-ray specular reflectivity and surface diffuse x-ray scattering. Unlike prior reflectivity-based studies, these measurements access both the time- and the length-scales of the evolution of the surface morphology during growth. In particular, we show that this technique allows direct measurements of the diffusivity for both inter- and intra-layer transport. Our results explicitly limit the possible role of island break-up, demonstrate the key roles played by nucleation and coarsening in PLD, and place an upper"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"0910.3601","kind":"arxiv","version":2},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}