{"paper":{"title":"Graphene formed on SiC under various environments: Comparison of Si-face and C-face","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"Guowei He, Luxmi, N. Srivastava, P. C. Mende, R. M. Feenstra, Yugang Sun","submitted_at":"2011-09-06T16:38:06Z","abstract_excerpt":"The morphology of graphene on SiC {0001} surfaces formed in various environments including ultra-high vacuum, 1 atm of argon, and 10^-6 to 10^-4 Torr of disilane is studied by atomic force microscopy, low-energy electron microscopy, and Raman spectroscopy. The graphene is formed by heating the surface to 1100 - 1600 C, which causes preferential sublimation of the Si atoms. The argon atmosphere or the background of disilane decreases the sublimation rate so that a higher graphitization temperature is required, thus improving the morphology of the films. For the (0001) surface, large areas of mo"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1109.1224","kind":"arxiv","version":2},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}