1D YIG hole-based magnonic nanocrystal

1 Pith paper cite this work. Polarity classification is still indexing.

1 Pith paper citing it
abstract

Magnetic media with artificial periodic modulation-magnonic crystals (MCs) - enable tunable spin-wave dynamics and band structure engineering. Nanoscaling enhances these capabilities, making magnonic nanocrystals promising for both fundamental studies and applications. Here, we report on the design, fabrication, and characterization of one-dimensional YIG MCs with nanoholes ($d \approx $ 150 nm) spaced $a \approx 1 \mu$m apart. Micro-focused Brillouin light scattering and propagating spin-wave spectroscopy, supported by TetraX and MuMax$^3$ simulations, reveal spin-wave transmission over 5 $\mu$m in the Damon-Eshbach configuration, and the formation of pronounced band gaps with rejection levels up to 26 dB. Detailed analysis of the spin-wave dispersion uncovered complex mode interactions, including two prominent anticrossings at 3.1 and 18.7 rad/$\mu$m, between which the spin-wave energy is predominantly carried by the $n$ = 2 mode, enabling efficient transmission. The results advance the development of functional MCs and open pathways toward 2D magnonic nanoarrays and magnonic RF nanodevices.

citation-role summary

background 1

citation-polarity summary

years

2025 1

verdicts

CONDITIONAL 1

roles

background 1

polarities

unclear 1

representative citing papers

Exchange spin-wave propagation in Ga:YIG nanowaveguides

cond-mat.other · 2025-09-05 · conditional · novelty 6.0

Spin waves in Ga:YIG nanowaveguides propagate at up to 600 m/s nearly independent of waveguide width, with decay lengths of 7 to 10 micrometers, several times faster than in YIG.

citing papers explorer

Showing 1 of 1 citing paper.

  • Exchange spin-wave propagation in Ga:YIG nanowaveguides cond-mat.other · 2025-09-05 · conditional · none · ref 22 · internal anchor

    Spin waves in Ga:YIG nanowaveguides propagate at up to 600 m/s nearly independent of waveguide width, with decay lengths of 7 to 10 micrometers, several times faster than in YIG.