Thermal conductivity in HFCVD diamond films on SiC increases from ~60 to ~200 W m^{-1} K^{-1} with depth due to grain coarsening, reconstructed via square-pulsed thermometry.
Lu, Functional Diamond 2 (1), 119-141 (2022)
1 Pith paper cite this work. Polarity classification is still indexing.
1
Pith paper citing it
fields
cond-mat.mtrl-sci 1years
2026 1verdicts
UNVERDICTED 1representative citing papers
citing papers explorer
-
Depth-Resolved Thermal Conductivity of HFCVD Diamond Films via Square-Pulsed Thermometry
Thermal conductivity in HFCVD diamond films on SiC increases from ~60 to ~200 W m^{-1} K^{-1} with depth due to grain coarsening, reconstructed via square-pulsed thermometry.