Compocasting parameter sweeps identify 400 rpm, 590°C, and 30 min as optimal for tensile properties in A356-10%SiCp composites, with particle distribution uniformity outweighing porosity effects.
Effects of casting temperature on the microstructure and wear resistance of compocast A356/SiCp composites: A comparison between SS and SL routes [J]