Nanoporous tantalum from liquid metal dealloying follows Gibson-Ashby scaling in elastic modulus (10-30 GPa) and hardness (0.3-1.1 GPa) due to enhanced ligament connectivity enabled by the CuBi dealloying bath.
Title resolution pending
1 Pith paper cite this work. Polarity classification is still indexing.
1
Pith paper citing it
fields
cond-mat.mtrl-sci 1years
2026 1verdicts
CONDITIONAL 1representative citing papers
citing papers explorer
-
Mechanical Scaling Laws and Deformation Behavior of Nanoporous Tantalum Microparticles
Nanoporous tantalum from liquid metal dealloying follows Gibson-Ashby scaling in elastic modulus (10-30 GPa) and hardness (0.3-1.1 GPa) due to enhanced ligament connectivity enabled by the CuBi dealloying bath.