Amorphous V2O3+p thin films (p = 0.05, 0.23, 0.49) show room-temperature ferromagnetism with about 14 kA/m saturation magnetization, tunable by oxygen content.
weak ferromagnetism
1 Pith paper cite this work. Polarity classification is still indexing.
1
Pith paper citing it
fields
cond-mat.mtrl-sci 1years
2024 1verdicts
CONDITIONAL 1representative citing papers
citing papers explorer
-
Control of ferromagnetism of Vanadium Oxide thin films by oxidation states
Amorphous V2O3+p thin films (p = 0.05, 0.23, 0.49) show room-temperature ferromagnetism with about 14 kA/m saturation magnetization, tunable by oxygen content.