CVD-grown Er:Y2O3 films show substrate-dependent texture, including epitaxy on YSZ and 99% (111) texture on an MBE oxide/Si template, with telecom inhomogeneous linewidths of 9 to 14 GHz.
The yttrium and erbium precursors were Y(tmhd) 3 and Er(tmhd)3 (where “tmhd” accounts for tetra-methyl-heptane-dionate)
1 Pith paper cite this work. Polarity classification is still indexing.
1
Pith paper citing it
fields
cond-mat.mtrl-sci 1years
2024 1verdicts
ACCEPT 1representative citing papers
citing papers explorer
-
Erbium doped yttrium oxide thin films grown by chemical vapour deposition for quantum technologies
CVD-grown Er:Y2O3 films show substrate-dependent texture, including epitaxy on YSZ and 99% (111) texture on an MBE oxide/Si template, with telecom inhomogeneous linewidths of 9 to 14 GHz.