PLD and ALD amorphous alumina microcantilevers exhibit bending plasticity with >10% strain at room temperature while sputtered films fail brittly; all show fracture toughness of 3.1 MPa m^{0.5} with no crack-tip plasticity.
Title resolution pending
2 Pith papers cite this work. Polarity classification is still indexing.
2
Pith papers citing it
citation-role summary
background 1
citation-polarity summary
verdicts
UNVERDICTED 2roles
background 1polarities
background 1representative citing papers
Oxygen plasma treatment on Ge heterostructures reduces interface trap density from the Si cap, improving mobility and lowering percolation density in 2DHGs compared with HF etching.
citing papers explorer
-
Microscale bending plasticity and fracture behavior of amorphous aluminum oxide films
PLD and ALD amorphous alumina microcantilevers exhibit bending plasticity with >10% strain at room temperature while sputtered films fail brittly; all show fracture toughness of 3.1 MPa m^{0.5} with no crack-tip plasticity.
-
Impact of surface treatments on the transport properties of germanium 2DHGs
Oxygen plasma treatment on Ge heterostructures reduces interface trap density from the Si cap, improving mobility and lowering percolation density in 2DHGs compared with HF etching.