Activation Energy of Metastable Amorphous Ge2Sb2Te5 from Room Temperature to Melt
pith:PXLEDI4A Add to your LaTeX paper
What is a Pith Number?\usepackage{pith}
\pithnumber{PXLEDI4A}
Prints a linked pith:PXLEDI4A badge after your title and writes the identifier into PDF metadata. Compiles on arXiv with no extra files. Learn more
read the original abstract
Resistivity of metastable amorphous Ge2Sb2Te5 (GST) measured at device level show an exponential decline with temperature matching with the steady-state thin-film resistivity measured at 858 K (melting temperature). This suggests that the free carrier activation mechanisms form a continuum in a large temperature scale (300 K - 858 K) and the metastable amorphous phase can be treated as a super-cooled liquid. The effective activation energy calculated using the resistivity versus temperature data follow a parabolic behavior, with a room temperature value of 333 meV, peaking to ~377 meV at ~465 K and reaching zero at ~930 K, using a reference activation energy of 111 meV (3kBT/2) at melt. Amorphous GST is expected to behave as a p-type semiconductor at Tmelt ~ 858 K and transitions from the semiconducting-liquid phase to the metallic-liquid phase at ~ 930 K at equilibrium. The simultaneous Seebeck (S) and resistivity versus temperature measurements of amorphous-fcc mixed-phase GST thin-films show linear S-T trends that meet S = 0 at 0 K, consistent with degenerate semiconductors, and the dS/dT and room temperature activation energy show a linear correlation. The single-crystal fcc is calculated to have dS/dT = 0.153 {\mu}V/K for an activation energy of zero and a Fermi level 0.16 eV below the valance band edge.
This paper has not been read by Pith yet.
discussion (0)
Sign in with ORCID, Apple, or X to comment. Anyone can read and Pith papers without signing in.