Pith. sign in

REVIEW

{\alpha}-FeAs-free SmFeAsO1-xFx by low temperature sintering with slow cooling

Not yet reviewed by Pith; the record is open.

This paper has not been read by Pith yet. Machine review is queued; the pith claim, tier, and objections will appear here once it completes.

SPECIMEN: schema-true, not a live event

T0 review · schema-true

One-sentence machine reading of the paper's core claim.

pith:XXXXXXXX · record.json · timestamp

arxiv 1303.1309 v2 pith:IXKW2G47 submitted 2013-03-06 cond-mat.supr-con

classification cond-mat.supr-con
keywords coolingsmfeaso1-xfxtemperaturefluorinesinteringslowconcentrationduring
verification ladder T0 review T1 audit T2 compute T3 formal
0 comments
read the original abstract

We obtained amorphous-FeAs-free SmFeAsO1-xFx using a low temperature sintering with slow cooling. SmFeAsO1-xFx is sintered at 980 {\deg}C for 40 hours and cooled slowly down to 600 {\deg}C. The low temperature sintering suppresses the formation of amorphous FeAs, and the slow cooling introduces much fluorine into SmFeAsO1-xFx. The superconductivity of this sample appears at 57.8 K and the superconducting volume fraction reaches 96 %. To study the change of fluorine concentration during the cooling process, samples are quenched by water at 950 {\deg}C, 900 {\deg}C, 850 {\deg}C, 800 {\deg}C, 750 {\deg}C and 700 {\deg}C. It is found that fluorine is substituted not only at the maximum heating temperature but also during the cooling process. The low temperature sintering with slow cooling is very effective to obtain a homogeneous SmFeAsO1-xFx with high fluorine concentration.