The potential of bulk black-phosphorus for thermoelectric applications has been experimentally studied. The Seebeck Coefficient (S) has been measured in the temperature range from 300 K to 385 K, finding a value of S = +335 +- 10 uV/K at room temperature (indicating a naturally occurring p-type conductivity). S increases with temperature, as expected for p-type semiconductors, which can be attributed to an increase of the charge carrier density. The electrical resistance drops up to a 40 % while heating in the studied temperature range. As a consequence, the power factor at 385 K is 2.7 times higher than that at room temperature. This work demonstrates the feasibility of black-phosphorus in thermoelectric applications, such as thermal energy scavenging, which typically require devices with high performance at temperatures above room temperature.

This paper has not been read by Pith yet.

discussion (0)

Sign in with ORCID, Apple, or X to comment. Anyone can read and Pith papers without signing in.