First Principles Study of Intrinsic and Extrinsic Point Defects in Monolayer WSe2

Not yet reviewed by Pith; the record is open.

This paper has not been read by Pith yet. Machine review is queued; the pith claim, tier, and objections will appear here once it completes.

SPECIMEN: schema-true, not a live event

T0 review · schema-true

One-sentence machine reading of the paper's core claim.

pith:XXXXXXXX · record.json · timestamp

arxiv 1901.05238 v1 pith:5ROXTAR7 submitted 2019-01-16 cond-mat.mtrl-sci

classification cond-mat.mtrl-sci
keywords defectsintrinsicpointsevacstateswse2siteenergies
verification ladder T0 review T1 audit T2 compute T3 formal

Signed reviews

No signed human review yet.

0 comments
read the original abstract

We present a detailed first principles density functional theory study of intrinsic and extrinsic point defects in monolayer (ML) WSe2. Among the intrinsic point defects, Se vacancies (Sevac) have the lowest formation energy (disregarding Se adatoms that can be removed with annealing). The defects with the next smallest formation energies (at least 1 eV larger) are SeW (Se substituting W atoms in an antisite defect), Wvac (W vacancies) and 2Sevac (Se divacancies). All these intrinsic defects have gap states that are not spin-polarized. The presence of a graphite substrate does not change the formation energies of these defects significantly. For the extrinsic point defects, we focus on O, O2, H, H2 and C interacting with perfect WSe2 and its intrinsic point defects. The preferred binding site in perfect WSe2 is the interstitial site for atomic O, H and C. These interstitial defects have no gap states. The gap states of the intrinsic defects are modified by interaction with O, O2, H, H2 and C. In particular, the gap states of Sevac and 2Sevac are completely removed by interaction with O and O2. This is consistent with the significantly larger stability of O-related defects compared to H- and C-related defects. The preferred binding site for O is Sevac, while that for H is SeW. H bonded to SeW results in spin-polarized gap states, which may be useful in defect engineering for spintronics applications. The charge transition levels and ionization energies of these defects are also computed. H in the interstitial site is an effective donor, while all the other defects are deep donors or acceptors in isolated WSe2 ML.

Discussion (0). Continue with ORCID to comment.

Forward citations

Cited by 2 Pith papers

Reviewed papers in the Pith corpus that reference this work. Sorted by Pith novelty score. Full citation record

  1. Long lived localized defect states in monolayer WSe$_2$: Optical Lifetime distribution and thermal evolution

    cond-mat.mtrl-sci 2026-07 conditional novelty 6.0 of 10

    Monolayer WSe2 defect photoluminescence at 4–120 K contains a ~0.5 ns exponential plus two 1/(t+τ) power-law tails (τ≈9 ns and ≈376 ns) attributable to distributed localized-state lifetimes.

  2. Defect-induced multiferroicity in bulk solid solutions of WSe$_2$ and WTe$_2$

    cond-mat.mtrl-sci 2026-03 unverdicted novelty 6.0 of 10

    Chalcogen vacancies in W(Se1-xTex)2 bulk crystals induce switchable ferroelectricity and ferromagnetism, producing multiferroic behavior at high vacancy concentrations while tellurium fraction drives a structural transition.

Pith tools