Influence by zirconium plastic deformation at temperature of 4.2 K on zirconium crystal lattice structure and magnitude of superconducting transition temperature Tc

classification ❄️ cond-mat.supr-con cond-mat.mtrl-scicond-mat.other
keywords temperaturezirconiumcrystaldeformationmagnitudegratingplasticstructure
0
0 comments X
read the original abstract

We have researched the effect of the zirconium deformation by the extension at the temperature of 4.2 K, with the subsequent heating up to the room temperature of 300 K, on both the zirconium crystal grating structure and the magnitude of superconducting transition temperature Tc, using the zirconium samples, synthesized by the method of the electron beam melting. In our opinion, a registered substantial increase of the critical temperature Tc (by 20%) is a result of both the superconductivity enhancement in the plastic deformation regions at the twin boundaries of the zirconium crystal grating and the effective change of the inter-electron attraction constant magnitude.

This paper has not been read by Pith yet.

discussion (0)

Sign in with ORCID, Apple, or X to comment. Anyone can read and Pith papers without signing in.